dc.description.abstractThe current paper has the objective to analyze the residual tension profile on the welded joints of the API 5L X65 steel, on the transversal and longitudinal directions, identifying the critical points close to the root face and the weld face. For this study two wending processes were used in the specimens: For the root pass it was used the Shield Metal Arc Welding (SMAW) process. For the hot passes, the filling passes and the cover pass it was used was the Gas Metal Arc Welding (GMAW) process. After the obtainment of the specimens the residual tensions were analyzed by the X-Ray diffraction method. It was observed for the transversal direction an inversion of the p residual tensions profile, furthermore, the same was observed for the longitudinal direction. On the root pass there was a predominant tractive profile for the transversal direction with tensions up to 280 Mpa, those were reverted to compressive tensions on the order of 165 Mp. For the longitudinal direction the traction tensions of 400 Mpa were inverted in compression tension on the order of 125 Mpa. The tension profile generated near the face of the weld did not suffer from tractive to compressive inversion. The critical points are mainly located by a distance between 4 to 8 mm from the central fusion line.pt_BR
dc.description.provenanceSubmitted by Rosa Sylvana Mousinho (syllmouser@biblioteca.ufpb.br) on 2019-02-28T12:38:36Z No. of bitstreams: 2 license_rdf: 805 bytes, checksum: c4c98de35c20c53220c07884f4def27c (MD5) Arquivototal.pdf: 3532205 bytes, checksum: e886de5346d427e5f18d89d8e06186b0 (MD5)en
dc.description.provenanceMade available in DSpace on 2019-02-28T12:38:36Z (GMT). No. of bitstreams: 2 license_rdf: 805 bytes, checksum: c4c98de35c20c53220c07884f4def27c (MD5) Arquivototal.pdf: 3532205 bytes, checksum: e886de5346d427e5f18d89d8e06186b0 (MD5) Previous issue date: 2018-06-12en
dc.description.sponsorshipCoordenação de Aperfeiçoamento de Pessoal de Nível Superior - CAPESpt_BR
dc.languageporpt_BR
dc.publisherUniversidade Federal da Paraíbapt_BR
dc.rightsAcesso abertopt_BR
dc.rightsAttribution-NoDerivs 3.0 Brazil*
dc.rights.urihttp://creativecommons.org/licenses/by-nd/3.0/br/*
dc.subjectSoldagempt_BR
dc.subjectAço API 5L X65pt_BR
dc.subjectTensões residuaispt_BR
dc.subjectDifração de raio-Xpt_BR
dc.subjectDireções longitudinal e transversalpt_BR
dc.subjectWeldingpt_BR
dc.subjectAPI 6L X65 Steelpt_BR
dc.subjectResidual tensionpt_BR
dc.subjectX-Ray diffractionpt_BR
dc.subjectLongitudinal and transversal directionspt_BR
dc.subjectSoldagem - Açopt_BR
dc.subjectTensão residualpt_BR
dc.subjectJunta soldada - tenacidadept_BR
dc.titleEstudo da evolução do perfil de tensões residuais em solda multipasse do aço API 5L X65pt_BR
dc.typeDissertaçãopt_BR
dc.contributor.advisor1Silva, José Hilton Ferreira da-
dc.contributor.advisor1Latteshttp://lattes.cnpq.br/3246011065909437pt_BR
dc.creator.Latteshttp://lattes.cnpq.br/9382465013246908pt_BR
dc.description.resumoO presente trabalho tem por objetivo analisar o perfil de tensões residuais nas juntas soldadas do aço API 5L X65, nas direções transversais e longitudinais, identificando os pontos críticos próximos a face da raiz e a face da solda. Para isso, as peças foram soldadas com dois processos: passe de raiz efetuado com o processo SMAW – Shield Metal Arc Welding e os passes quente, enchimento e acabamento com o processo GMAW – Gas Metal Arc Welding. Após a obtenção dos corpos de prova, as tensões residuais foram analisadas pelo método da difração residual. Foi observado, para a direção transversal, uma inversão no perfil de tensões residuais. O mesmo foi observado para a direção longitudinal. No passe de raiz, tinha-se um perfil predominantemente trativo, com tensões de até 280 MPa, que foram revertidas para tensões compressivas, na ordem de 165 MPa para a direção transversal. Para a direção longitudinal, tensões de tração da ordem de 400 MPa foram invertidas em tensões de compressão da ordem de 125 MPa, já o perfil de tensões gerado próximo a face da solda não sofreu inversão de trativa para compressiva. Os pontos críticos estão predominantemente situados a uma distância entre 4 e 8 mm da linha central de fusão.pt_BR
dc.publisher.countryBrasilpt_BR
dc.publisher.departmentEngenharia Mecânicapt_BR
dc.publisher.programPrograma de Pós-Graduação em Engenharia Mecânicapt_BR
dc.publisher.initialsUFPBpt_BR
dc.subject.cnpqCNPQ::ENGENHARIAS::ENGENHARIA MECANICApt_BR
Aparece nas coleções:Centro de Tecnologia (CT) - Programa de Pós-Graduação em Engenharia Mecânica

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
Arquivototal.pdfArquivo total3,45 MBAdobe PDFVisualizar/Abrir


Este item está licenciada sob uma Licença Creative Commons Creative Commons