dc.description.abstractThe development of manufacturing processes that combine low cost and efficiency in the production of complex quasicrystalline metal alloys has become a challenge for researchers and engineers in order to make their production viable in industrial applications. The quasicrystalline alloys have unique microstructural characteristics and differentiated properties that make them candidates for potential uses in coatings and composites of ductile matrixes, catalysts, among others. Despite the special characteristics of these alloys, coupled with the low cost of the raw materials, the metallurgy to obtain them needs adequate processing conditions. Several conventional manufacturing techniques are used to obtain quasicrystalline alloys, such as: conventional casting in induction furnace, fast cooling casting, powder metallurgy, among others. Manufacturing processes using fast cooling showed to be efficient in the production of these materials with a higher fraction of quasicrystalline phases, already in the first stage of processing. Most of these techniques, however, present as major drawbacks high costs for large-scale production. In this sense, it is proposed a smelter processing route via unidirectional solidification, whereby the severity of the cooling can be increased in order to maximize the quasicrystalline phase amount. For this purpose, the alloy with nominal composition Al62.5Cu25Fe12.5 was unidirectionally fused and solidified under optimized processing conditions, it was possible to produce an alloy with more than 70% quasicrystalline phase, still in the melting stage. With the heat treatment of homogenization by 750 ° C / 2h, it was possible to produce 500g of alloy with more than 90% of quasicrystalline phase. This result was efficient when compared to already established techniques of use. It was possible, at the end of the work, to create an efficient route, with optimized processing conditions, for the production of quasicrystalline alloys practically homogeneous, with great prospect of large-scale production.pt_BR
dc.description.provenanceSubmitted by Nataly Leite (nataly@biblioteca.ufpb.br) on 2021-01-13T20:21:57Z No. of bitstreams: 2 license_rdf: 805 bytes, checksum: c4c98de35c20c53220c07884f4def27c (MD5) ThayzaPachecoDosSantosBarros_Tese.pdf: 14552497 bytes, checksum: 413d9ab02d1735155811f621f9ae0cf5 (MD5)en
dc.description.provenanceApproved for entry into archive by Biblioteca Digital de Teses e Dissertações BDTD (bdtd@biblioteca.ufpb.br) on 2021-02-11T04:18:24Z (GMT) No. of bitstreams: 2 license_rdf: 805 bytes, checksum: c4c98de35c20c53220c07884f4def27c (MD5) ThayzaPachecoDosSantosBarros_Tese.pdf: 14552497 bytes, checksum: 413d9ab02d1735155811f621f9ae0cf5 (MD5)en
dc.description.provenanceMade available in DSpace on 2021-02-11T04:18:24Z (GMT). No. of bitstreams: 2 license_rdf: 805 bytes, checksum: c4c98de35c20c53220c07884f4def27c (MD5) ThayzaPachecoDosSantosBarros_Tese.pdf: 14552497 bytes, checksum: 413d9ab02d1735155811f621f9ae0cf5 (MD5) Previous issue date: 2019-05-30en
dc.description.sponsorshipConselho Nacional de Pesquisa e Desenvolvimento Científico e Tecnológico - CNPqpt_BR
dc.languageporpt_BR
dc.publisherUniversidade Federal da Paraíbapt_BR
dc.rightsAcesso embargadopt_BR
dc.rights.urihttp://creativecommons.org/licenses/by-nd/3.0/br/*
dc.subjectSolidificação direcionalpt_BR
dc.subjectQuasicristalpt_BR
dc.subjectUnidirecionalpt_BR
dc.subjectDirectionalpt_BR
dc.subjectQuasicrystallinept_BR
dc.subjectUnidirectionalpt_BR
dc.titleOtimização dos parâmetros de fundição via solidificação direcional na obtenção de ligas metálicas complexas quasicristalinas de base alumíniopt_BR
dc.typeTesept_BR
dc.contributor.advisor1Cavalcante, Danielle Guedes de Lima-
dc.contributor.advisor1Latteshttp://lattes.cnpq.br/2575577028682912pt_BR
dc.contributor.advisor-co1Lima, Bruno Alessandro Silva Guedes de-
dc.contributor.advisor-co1Latteshttp://lattes.cnpq.br/2232828745401224pt_BR
dc.creator.Latteshttp://lattes.cnpq.br/8514875145972598pt_BR
dc.description.resumoO desenvolvimento de processos de fabricação que aliem baixo custo e eficiência na produção de ligas metálicas complexas quasicristalinas, tornou-se um desafio para pesquisadores e engenheiros de modo a tornar sua produção viável em aplicações industriais. As ligas quasicristalinas apresentam características microestruturais singulares e propriedades diferenciadas que as tornam candidatas a usos potenciais em revestimentos e compósitos de matrizes dúcteis, catalizadores, entre outros. Apesar das características especiais destas ligas, atreladas ao baixo custo das matérias-primas, a metalurgia para sua obtenção necessita de condições adequadas de processamento. Várias técnicas convencionais de fabricação são usadas na obtenção de ligas quasicristalinas, tais como: fundição convencional em forno de indução, fundição por resfriamento rápido, metalurgia do pó, entre outras. Os processos de fabricação que usam resfriamento rápido mostraram-se eficientes na produção destes materiais com uma maior fração de fases quasicristalinas, já na primeira etapa do processamento. A maioria destas técnicas, porém, apresenta como principais inconvenientes altos custos para produção em larga escala. Neste sentido, propõese uma rota de processamento de fundição via solidificação unidirecional, onde se poderá aumentar a severidade do resfriamento de modo a maximizar a quantidade de fase quasicristalina. Para tanto, a liga com composição nominal Al62,5Cu25Fe12,5 foi fundida e solidificada unidirecionalmente sob condições otimizadas do processamento, sendo possível a produção de uma liga com mais de 70% de fase quasicristalina, ainda na etapa de fundição. Com o tratamento térmico de homogeneização por 750°C/2h, foi possível produção de 500g de liga com mais de 90% de fase quasicristalina. Este resultado mostrou-se eficiente quando comparado a técnicas de uso já consagradas. Foi possível, assim, ao final do trabalho criar uma rota eficaz, com condições otimizadas de processamento, para produção de ligas quasicristalinas praticamente homogêneas, com grande perspectiva de produção ampla.pt_BR
dc.publisher.countryBrasilpt_BR
dc.publisher.departmentEngenharia Mecânicapt_BR
dc.publisher.programPrograma de Pós-Graduação em Engenharia Mecânicapt_BR
dc.publisher.initialsUFPBpt_BR
dc.subject.cnpqCNPQ::ENGENHARIAS::ENGENHARIA MECANICApt_BR
Aparece nas coleções:Centro de Tecnologia (CT) - Programa de Pós-Graduação em Engenharia Mecânica

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
ThayzaPachecoDosSantosBarros_Tese.pdf14,21 MBAdobe PDFVisualizar/Abrir    Solicitar uma cópia


Este item está licenciada sob uma Licença Creative Commons Creative Commons