dc.description.abstractCuAlMn alloys are quite attractive to various applications due to their unique properties of form memory effect (SME) and overelasticity (SE). Thus, there is a continuous interest in SMAs based on Cu due to its low cost, pronounced thermal conductivity, good processability, as well as the highly cushioned properties, also combined with their elastocalorimetry properties. However, these alloys have their limitations associated with their high fragility which is attributed to high elastic anisotropy, ordered phase formation and rude grain formation. In this work, we seek to improve the properties by applying the process of hot and cold rolling in a CuAl17Mn9Cr2 alloy. This alloy was elaborated in an induction oven in the form of rectangular ingots. The formation of a microstructure was observed the Beta and Alpha phases, as well as chromium -rich intermetallic compounds with a fewer Mn presence. This alloy can easily be rolled into room temperature. Cyclic traction testing tests showed the reach of a 5 % overlap.pt_BR
dc.description.provenanceSubmitted by Fernando Augusto Alves Vieira (fernandovieira@biblioteca.ufpb.br) on 2023-08-24T10:50:13Z No. of bitstreams: 2 license_rdf: 805 bytes, checksum: c4c98de35c20c53220c07884f4def27c (MD5) FranciscoWlaudyErimarLourençoDeAraújoJunior_Dissert.pdf: 4958204 bytes, checksum: b6e42848d51dd45f33f7ffd9f14f7cee (MD5)en
dc.description.provenanceMade available in DSpace on 2023-08-24T10:50:13Z (GMT). No. of bitstreams: 2 license_rdf: 805 bytes, checksum: c4c98de35c20c53220c07884f4def27c (MD5) FranciscoWlaudyErimarLourençoDeAraújoJunior_Dissert.pdf: 4958204 bytes, checksum: b6e42848d51dd45f33f7ffd9f14f7cee (MD5) Previous issue date: 2022-08-31en
dc.description.sponsorshipCoordenação de Aperfeiçoamento de Pessoal de Nível Superior - CAPESpt_BR
dc.languageporpt_BR
dc.publisherUniversidade Federal da Paraíbapt_BR
dc.rightsAcesso embargadopt_BR
dc.rightsAttribution-NoDerivs 3.0 Brazil*
dc.rights.urihttp://creativecommons.org/licenses/by-nd/3.0/br/*
dc.subjectEngenharia Mecânicapt_BR
dc.subjectLigas Cu-Al-Mn-Crpt_BR
dc.subjectSuperelasticidadept_BR
dc.subjectComposto intermetálicopt_BR
dc.subjectMechanical Engineeringpt_BR
dc.subjectCuAlMnCr alloyspt_BR
dc.subjectSuperelasticitypt_BR
dc.subjectIntermetallic compoundpt_BR
dc.titleEfeito do tratamento termomecânico na microestrutura e propriedades mecânicas da ligA CuAl17Mn9 contendo 2.0 at% de cromopt_BR
dc.typeDissertaçãopt_BR
dc.contributor.advisor1Gomes, Rodinei Medeiros-
dc.contributor.advisor1Latteshttp://lattes.cnpq.br/2571715314037365pt_BR
dc.creator.Latteshttp://lattes.cnpq.br/8659839954645809pt_BR
dc.description.resumoLigas CuAlMn são bastante atraentes para diversas aplicações devido às suas propriedades únicas de efeito de memória de forma (SME) e superelasticidade (SE). Assim, existe um interesse contínuo em SMEs baseados em Cu devido ao seu baixo custo, condutividade térmica pronunciada, boa processabilidade, bem como, as propriedades de alta capacidade de amortecimento, combinado também com suas propriedades de elastocalorimetria. Porém, estas ligas tem suas limitações associadas à sua alta fragilidade a qual é atribuída a alta anisotropia elástica, formação de fases ordenadas e formação de grão grosseiros. Neste trabalho busca-se a melhoria das propriedades aplicando o processo de laminação a quente e a frio em uma liga CuAl17Mn9Cr2. Esta liga foi elaborada em forno de indução na forma de lingotes retangulares. Foi observado a formação de uma microestrutura as fases beta e alfa, bem como, compostos intermetálicos ricos em cromo com presença menor quantidade de Mn. Esta liga pode ser laminada facilmente a temperatura ambiente. Os testes de ensaios de tração cíclicos mostraram o alcance de uma superelasticidade da ordem de 5 %.pt_BR
dc.publisher.countryBrasilpt_BR
dc.publisher.departmentEngenharia Mecânicapt_BR
dc.publisher.programPrograma de Pós-Graduação em Engenharia Mecânicapt_BR
dc.publisher.initialsUFPBpt_BR
dc.subject.cnpqCNPQ::ENGENHARIAS::ENGENHARIA MECANICApt_BR
Aparece nas coleções:Centro de Tecnologia (CT) - Programa de Pós-Graduação em Engenharia Mecânica



Este item está licenciada sob uma Licença Creative Commons Creative Commons